Environmental behavior and stress corrosion characteristics of nano/sub-micron E950 Aluminum alloy

Eli Aghion, Lnbar Guinguis

Research output: Contribution to journalArticlepeer-review

5 Scopus citations

Abstract

The corrosion performance and stress corrosion resistance of E950 Aluminum alloy with nano/sub-micron structure were evaluated in 3.5% NaCl solution. The results obtained indicated that the corrosion and stress corrosion resistance of E950 alloy were relatively reduced compared to that of the conventional coarse-grained alloy (Al-4.65%Mg). In particular, the inherently improved ultimate tensile strength of E950 alloy was significantly decreased under stress corrosion conditions.

Original languageEnglish
Pages (from-to)920-924
Number of pages5
JournalAdvanced Engineering Materials
Volume11
Issue number11
DOIs
StatePublished - 1 Jan 2009

Fingerprint

Dive into the research topics of 'Environmental behavior and stress corrosion characteristics of nano/sub-micron E950 Aluminum alloy'. Together they form a unique fingerprint.

Cite this