STRESS CORROSION OF TYPE 304 STEEL IN H//2SO//4 ALKALI HALIDE ENVIRONMENTS.

D. Eliezer, P. Pinkus, D. Itzhak

Research output: Contribution to conferencePaperpeer-review

1 Scopus citations
Original languageEnglish
Pages193-199
Number of pages7
StatePublished - 1 Dec 1981