Original language | English |
---|---|
Pages (from-to) | 348-350 |
Number of pages | 3 |
Journal | Soviet Materials Science |
Volume | 1 |
Issue number | 4 |
DOIs | |
State | Published - 1 Jul 1966 |
Externally published | Yes |