Superalloys and Refractory Metals: The Oxidation Resistance of Sintered W-Cr-Pd Alloys
- A Makonovitsky
- , R Shneck
- , S Hessel
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution › peer-review