Corrosion and Stress Corrosion Cracking of New Wrought Magnesium Alloys

Translated title of the thesis: קורוזיה וקורוזיית מאמצים של נתכי מגנזיום חשילים חדשים
  • Guy Yehuda Ben-Hamo

Student thesis: Doctoral Thesis

Date of Award2010
Original languageHebrew
Awarding Institution
  • Ben-Gurion University of the Negev
SupervisorDan Eliezer (Supervisor)